Here’s a couple of quick shots of a ring currently in progress. I de-sprued after casting and assembled the Pt top with its 18K Y shank. Virtually no cleanup other than that necessary to stick these together (with 18K solder) and you can still see solder gooped a bit around the seam. This ring was developed in Rhino and printed in two seperate components on the B9.